Phil,
If you are talking IPA vs Ethyl or methanol, the latter is much more
reactive to resin based fluxes, the other advantage is the 200 proof
denatured will also dehydrate the device it is used on. I was taught
in the Navy to use methanol exclusively. On the older formulations
of 60-40 or 63-37, I feel there is nothing better, it also has the
advantage as a de greaser so will remove fingerprints. When I wash a
board with ethyl I always position the board vertical and wash from the
center out. As a comparison using a spray on de-fluxer causes
moisture to condense on the board. Ethyl or methanol removes
moisture, it is for the most part anhydrous. If you purchase the 200
proof food grade version, one must pay the appropriate state and federal
taxes. There is a 200 proof, 1% denatured version that doesn't have
the tax issues, and there is a 190 proof, fuel grade but that leaves a
residue due to the denaturing agent.
pat goodyear
retired
On Fri, Apr 24, 2015 at 8:12 AM, Nutting, Phil wrote:
> We have had many posts regarding the ability of alcohol to evenly
> distribute flux and other contaminates over the surface of the board
> or part. Does methanol do that same thing?
>
> Phil Nutting | HVP Development Engineer | Excelitas Technologies
> Corp
>
> Lab: +1 978.224.4332 | Office: +1 978.224.4152
> 35 Congress St, Salem, MA 01970 USA
> [log in to unmask]<mailto:[log in to unmask]>
> www.excelitas.com<http://www.excelitas.com/>
>
>
> [Excelitas R_emailsig]
>
>
> Please consider the environment before printing this e-mail.
> ________________________________
> This email message and any attachments are confidential and
> proprietary to Excelitas Technologies Corp. If you are not the
> intended recipient of this message, please inform the sender by
> replying to this email or sending a message to the sender and destroy
> the message and any attachments. Thank you.
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|