interference fringe type might be work.
On May 9, 2015, at 4:16 AM, Lee Hitchens wrote:
> Thanks Louis
>
> I think the issue is the transulence of the coating. I think the
> measurement is done on glass slides for parylene. However,
> difficulties
> appear to occur with unclear coatings such as silicones.
>
> However, I will pursue this and check.
>
> Best Regards
>
> Dr Lee Hitchens
>
> SCH Technologies is a Division of SCH Services Limited
> Mob: +44 (0) 7862 25 33 21
> www.conformalcoating.co.uk <http://www.conformalcoating.co.uk/>
>
> TECHNICAL SUPPORT SERVICE
>
> SCH Services Ltd offers a Technical Support Helpline to help
> address all
> issues relating to reliability. This includes contamination testing,
> cleanliness and cleaning issues, plus any coating related questions.
> Please contact us via email or telephone:
>
> [log in to unmask] +44 (0)1226 249019 (office hours & answerphone)
> +44 (0)7862 253321(out-of-hours emergency)
>
> The opinions expressed in this e-mail are strictly those of the
> sender and
> not of SCH Services Limited. This communication may contain
> information
> which is confidential and may also be privileged. It is for the
> exclusive
> use of the intended recipient(s). Unauthorised use, copying or
> disclosure
> of any of it may be unlawful. If you are not the intended recipient(s)
> please note that any distribution, copying or use of this
> communication or
> the information in it is strictly prohibited. If you have received
> this
> communication in error please notify us by e-mail or by telephone (+44
> (0)1226 249019) and then delete the e-mail and any copies of it. Virus
> Warning - Although steps have been taken to ensure that all email and
> attachments are virus-free, we cannot guarantee nor be held liable.
>
> Company Registration: 04043334
> Registered office: SCH Services Limited Newburgh Building McLintock
> Way
> Barnsley South Yorkshire S70 6BF
>
>
>
>
>
>
>
> On 08/05/15 18:41, "Louis Hart" <[log in to unmask]> wrote:
>
>> Lee, it has been more than 15 years, but I measured synthetic diamond
>> coatings, with thickness a fraction of what I expect conformal
>> coating
>> should be, on metals with an ellipsometer and an instrument called a
>> 'Nanospec'. The ellipsometer was more accurate, as it measured the
>> material property (dielectric permittivity, I think it was) of the
>> specimen then used that to determine coating thickness. The
>> nanospec, if
>> my memory is correct, had a catalogue of material parameters from
>> which
>> you called up yours and got a thickness in one observational step.
>>
>> Both used a laser, again if my memory is correct. The area of
>> coating
>> being measured was a tiny spot, much smaller than any dimension of a
>> component leg I know of. Louis
>>
>>
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Lee Hitchens
>> Sent: Thursday, May 07, 2015 3:50 AM
>> To: [log in to unmask]
>> Subject: [TN] Conformal Coating Thickness Measurement on legs of
>> components
>>
>> Hi all
>>
>> I am being asked regularly now on options for measuring coating
>> thickness
>> on legs. I am trying to determine if there is actually a practical
>> solution?
>> Cost is less important compared to being a workable relatively quick
>> process?
>>
>> One thing that could be an issue is many times its a silicone
>> coating and
>> this tends to be less than clear optically. Some systems need clear
>> coatings to be successful.
>>
>> Has anyone had any success with this?
>>
>> Best Regards
>>
>> Dr Lee Hitchens
>>
>> SCH Technologies is a Division of SCH Services Limited
>>
>> Mob: +44 (0) 7862 25 33 21
>>
>> www.conformalcoating.co.uk <http://www.conformalcoating.co.uk/>
>>
>>
>>
>>
>>
>>
>> _____________________________________________________________________
>> _
>> This email has been scanned by the Symantec Email Security.cloud
>> service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> _____________________________________________________________________
>> _
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
> service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|