Paul,
I suggest you use any ESD safe material such as Durostone (Wave Solder
Fixture type material).
If you need any material or any tooling manufactured, please contact me off
line.
Chris Chapman
-----Original Message-----
From: Paul Stolar <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Thursday, September 17, 1998 4:20 PM
Subject: [TN] Re[2]: [TN] g10
>Content-Transfer-Encoding: 7bit
>
>
>
> We are going to use it for gauging leads. if it is not ESD, then we
> must use another material.
>
> Thanks
>
> Paul Stolar
>
>
>______________________________ Reply Separator
_________________________________
>Subject: Re: [TN] g10
>Author: [log in to unmask]> Chris Chapman
<[log in to unmask]
>at internet
>Date: 9/17/98 1:53 PM
>
>
>Paul,
>
> No!
> What is your intended use for the G10?
>
>Chris Chapman
>-----Original Message-----
>From: Paul Stolar <[log in to unmask]>
>To: [log in to unmask] <[log in to unmask]>
>Date: Thursday, September 17, 1998 2:08 PM
>Subject: [TN] g10
>
>
>> Here is a simple question I hope someone can answer for me.
>>
>> Is G10 ESD safe?
>>
>>################################################################
>>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>>################################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with
following
>text in the body:
>>To subscribe: SUBSCRIBE TechNet <your full name>
>>To unsubscribe: SIGNOFF TechNet
>>################################################################
>>Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section
>for additional information.
>>For technical support contact Hugo Scaramuzza at [log in to unmask] or
>847-509-9700 ext.312
>>################################################################
>>
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text
>in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for
>additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700
>ext.312
>################################################################
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|