TechNet, Bill Foran, fulrl @ Boeing
I am very surprised to hear about your problems with Shipley Electroless
Copper. I am with Electro Plate Circuitry in Carrollton, Tx. We
manufacture Military and High-Rel Commercial Multilayers. We have been
using Shipley # 3350 Electroless Line for the past 7 years. We have had
great success from a performance and support standpoint. We have found that
when we do run into a problem, Shipley's tech support is at our facility
within hours and solves the problem in a timely manner. We have always
found that the problem is a result of something we did or did not do. Feel
free to give me a call, If I cannot help you, I can put you in contact with
someone who can. (214)466-0818.
>Subject: Electroless copper
>From: [log in to unmask] at Internet
>Date: 6/12/96 7:41 AM
>
>
> We have recently changed our Electroless Chemistries and Electrolytic
> Copper to Shipley product line. We have been overwhelmed with scrap for
> voids, plating separations and adhesion problems. We have followed the
> vendor recommendations and are running within their guidelines. We need
> some technical help. The support we've been receiving is not getting us
> anywhere. Currently we are shut down for all production due to scrap
> levels. HELP!
>
> Thank you
===============================================================
Nicolas Garcia
V.P. Operations