TECHNET Archives

June 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Phil Bavaro <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Thu, 6 Jun 2013 20:11:20 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (40 lines)
Look up kapton labels    129-T1K

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Thursday, June 06, 2013 1:04 PM
To: [log in to unmask]
Subject: [TN] Labels that withstand Wavesolder with alcohol based flux

Hi All,



I know I have had PCB label issues not standing-up to alcohol based flux and wave solder in the past and have found some that worked...but because I'm so absent minded,  I forgot which ones they were.



The labels that we are using now are thermal transfer ink printed, they SAY that they can withstand wave soldering processes, but the adhesive is acrylic and the alcohol in the flux attacks the adhesive, and the labels wash off in our DI cleaner.



Anyone got a good recommendation for label stock?



Steve




______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
________________________________
 This message and any attachments are solely for the use of the addressee and may contain L-3 proprietary information that may also be defined as USG export controlled technical data. If you are not the intended recipient, any disclosure, use or distribution of its content is prohibited. Please notify the sender by reply e-mail and immediately delete this message and any attachments.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2