We have experienced minor wrinkling on a Dynachem Cut Sheet Laminator when the exit temperature rose above 50 deg C.  We lowered the temperature below 50 C and the problem went away.  Other than that, we have not seen any other problems with HG.


------------------------------------------------------------------------------------------------
Ed Wright - Tech. Service 	OS-TECH & PCB Supplies
Oliver Sales Company 	Phone:  (214) 231-1522
13445 Floyd Circle 	Fax:  (214) 644-3585
Dallas, Texas  75243-1595 	E-mail:  [log in to unmask]
------------------------------------------------------------------------------------------------

----------
From:  [log in to unmask][SMTP:[log in to unmask]]
Sent:  Monday, April 01, 1996 12:25 PM
To:  [log in to unmask]
Subject:  Dynachem Film Problems

Has anyone experienced problems with Dynachem HG film in the past 2-3 months?  Particularly wrinkling during lamination or tenting issues.  We have checked our Dynachem and DuPont Hot Roll Laminators and they appear OK.  I understand that Dynachem changed the thickness of Mylar and it seems to come off too easily.
Any comments would be appreciated.