TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Ingemar Hernefjord (KC/EMW)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord (KC/EMW)
Date:
Tue, 17 Aug 2004 09:16:26 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
Seal Science say they have it all: http://www.sealscience.com/html/products/VacuumCupsPdfs/15about.pdf
ultrahighvacuum guys use pure gold gaskets: http://www.sisweb.com/catalog/F39.pdf
ourselves, we use as simple as butyl rubber: http://www.allstategasket.com/materials.asp (not Ultravacuum, of course)
Butyl rubber group includes ordinary rubber used in your mountainbike tire, can keep vacuum or pressure for very long time.
/Ingemar


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Crepeau, Phil
Sent: den 17 augusti 2004 02:25
To: [log in to unmask]
Subject: Re: [TN] thin film


hi,

i believe you should be able to use a gasket material such as viton.

phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Douglas O. Pauls
Sent: Monday, August 16, 2004 2:02 PM
To: [log in to unmask]
Subject: [TN] thin film


Good day all,
I am in need of a recommendation for a thin film sealant material.  I need
it to be 15-20 mils thick, cuttable, and preferrably non silicone.  We have
considered the Sil-Pad technology, but as this will be used in a vacuum
seal operation, I am concerned about silicone outgassing or cross
contamination.  Are there any thin gasket materials from the engineered
rubbers that anyone would recommend?

Doug Pauls

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2