Correct. 20 uinches of nickel is not ENIG.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of George Milad
Sent: Thursday, March 15, 2007 11:05 AM
To: [log in to unmask]
Subject: Re: [TN] IPC ENIG SPECIFICATION
The ENIG specification 4552 specifies Ni at 120 - 240 uins and gold
minimum
2 uins typically 2- 5 uins.
Regards
George Milad
George Milad
Chairman IPC plating Committee
National Accounts Manager for Technology Uyemura International Corp
(UIC)
249 Town Line Rd
Southington CT 06489
[log in to unmask]
Cell: (516) 901 3874
************************************** AOL now offers free email to
everyone.
Find out more about what's free from AOL at http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------