The white paint pens we've been using to mark on PWB solder mask have been discontinued. These pens required only a room temperature solvent evaporation cure.
We've tried a couple of alternatives, but these have washed off with our wash chemistry. I'm looking for alternatives.
To maintain non-commercial forum, please send any specific recommendations to me offline.