Hi Wayne,
The kicker is the alkaline etch. If you were using acid etch, usually, the
chromates don't bother you much. I don't feel that just a sulfuric acid will
get the job done 100% of the time. Some companies are using a acid cleaner
with a slight microetch in it to remove the chromates. My preference is to
use a alkaline cleaner with a chromate removal chemistry in it, followed by a
good water rinse and dry. There are some alkaline etch dry films on the
market that are compatible with this type of preclean.
Ken Bridges - Morton
***************************************************************************