on Thu, 15 Aug 1996 18:12:57 -0400
"3.1415" <[log in to unmask]> asked:
>What was the baking temperature?
Curie temp was 120C so I baked at 130C.
[...]
>> De-aging of ceramic capacitors is a bake above their Curie point
>> temperature. I've had to bake caps anywhere from 1 to 16 hours to de-age
>> them. No vacuum is involved.
[...]
***************************************************************************