Hi Bill,
Just a few quick suggestions,
1. Is there any draft built into the mold? It would make ejecting the part a
lot easier.
2. Can you make the mold itself from a flexible material? This too would
make getting the parts out easier.
Hope this helps,
Mike Di Giacomo
WorldHeart Corp.
-----Original Message-----
From: Kasprzak, Bill (sys) USX [mailto:[log in to unmask]]
Sent: Monday, July 16, 2001 11:51 AM
To: [log in to unmask]
Subject: [TN] Recommendations for developing a mold
Hello all,
I am involved with a project that requires that I encapsulate a pc board in
mold so that when completed, it will be a ring with an ID of 1.37" and an OD
of 1.64". The ring will be .13" thick and .35" tall. There will be six, 28
AWG wires exiting the finished potted assembly. The potting compound will be
Emerson & Cumings 2651-40 with Catalyst 11.
I have a basic 3 piece mold that works OK, but the pieces only
reflect what the final product should look like. It takes a little work to
get the mold apart even though mold release is used. The cure for the
potting is 8 - 16 hours at 180 deg F
What I'm looking for is any tricks and hints that should be incorporated
into the mold design that would facilitate easy processing. What I mean is
to make it easier to pour the material, easy to assemble into the mold, easy
to take apart, etc. etc. Right now the whole process just seems to be crude
and messy. Maybe, that's just the nature of the beast.
Any and all responses appreciated. Thanks.
Bill Kasprzak
Moog Inc., Electronic Assembly Engineering
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|