The immersion white tin we have seen requested is Omikron by Florida CirTech
and I have heard of Dexter and Alphametal producing an immersion white tin.
Supposedly assemblers are moving to the IWT because it is more reworkable
than OSP, the surface co-planarity is good and so is the solderability.
We're trying to determine where the industry is going, is anyone else seeing
this happen?
On Thu, 1 Jun 2000 13:38:45 -0700 , Brooks Bill wrote:
> This is going to date me... I used to manufacture boards in my youth, we
> used electroless tin as a coating for boards where heavy hydro-squeegee
> solder coating was not required... Is this what you mean by white tin
> immersion?
> -Bill Brooks
>
> -----Original Message-----
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Thursday, June 01, 2000 12:18 PM
> To: [log in to unmask]
> Subject: [TN] Immersion White Tin
>
>
> I hope to generate some discussion on this subject, since there wasn't
much
> from last weeks questions on immersion white tin...
>
> We (as a PCB fabricator) have had several inquiries about immersion white
> tin from our customers, but we don't see any of the large OEM's making a
> move towards it.
> Any opinions out there?
>
>
>
>
>
>
>
> _______________________________________________________
> Get 100% FREE Internet Access powered by Excite
> Visit http://freelane.excite.com/freeisp
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following
> text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
_______________________________________________________
Get 100% FREE Internet Access powered by Excite
Visit http://freelane.excite.com/freeisp
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|