Hi!
150 mounted boards wait to be wave soldered.
50 siblings with the same date code already passed the process,but 15%
showed delamination.
The visual examination showed a lack of healthy black colour on the
inner
layer conductors,very different from the state of younger relatives from
the
same vendor.
Age: 4 months.
Number of layers:10
Prebake:none
Previous vendor history:good
What's the verdict for the survivers after soldering?
What should be done with the mounted boards?
Excuse please my nonscientific letter,and try to help!
Thank you,
Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|