I recommend that you look at Envirosense Envirogold 816 (contact Mark Palmer
408-894-9901) or Kyzen Aquanox SSA (800-845-5524).  Both are excellent
saponifiers and several of our clients use them successfully for low solids
flux residues.  Both are environmentally friendly.