Hi Gregg! There is a CTE table on page 36 of the JSTD-001 Handbook (table
4-12) which lists the CTE's of common assembly materials.
Dave Hillman
Rockwell Collins
[log in to unmask]
"Gregg A. Owens"
<owensMTTC@EARTHL
INK.NET> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
02/14/2006 04:46 [TN] Coeffecient of Thermal
PM Expansion (CTE) Rates
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
"Gregg A. Owens"
<owensMTTC@EARTHL
INK.NET>
Dear Technetters:
Anyone have a source for different CTE rates for common elements used in
electronic assemblies?
Any input appreciated.
Gregg A. Owens
Master IPC Instructor
Executive Director
Manufacturing Technology Training Center, Inc.
10427 San Sevaine Way, Suite 'I"
Mira Loma, CA 91752 USA
Tel (951) 360-1324 Fax (951) 360-1346
www.mttc-inc.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------