I have a question for Ron and three comments for Michael.
Ron,
If your situation wasn't a contamination issue what kind of an issue was it?
Michael,
1. It's almost impossible to mesure contamination on leads that when through
an assembly process because you can't tell if what you find was there to
start with or a result of the assembly material. You'll need to analyze
component leads before assembly.
2. Our experience indicates surface contamination seldom is the cause for
our solderability/soldering problems.
3. The "imprint" appearance you discribe shoulds a lot like what we call
"Foot-in-the-Mud" which we believe to be a combination of lead
solderability, solder paste activity, stencil print height, lead
coplanarity.
Regards,
George
George M. Wenger, DMTS Bell Laboratories Princeton
Supply Network Solutions
PO Box 900, Princeton NJ 08542-0900
Route 569 Carter Rd., Hopewell, NJ 08525
(609)-639-2769 (Office), 3210 (Lab), 2343 (Fax)
[log in to unmask]
-----Original Message-----
From: Hollandsworth, Ron [mailto:[log in to unmask]]
Sent: Friday, October 27, 2000 7:34 AM
To: [log in to unmask]
Subject: [TN] Re] Contamination of leads
Michael:
I had a similar situation on an Avionics project within the last year. The
customer's first thought was a contamination issue. We decided to bring in
a third party with the expertise to tell us what direction we needed to take
on the issue. I contacted Contamination Studies Labs (CSL) in Kokomo,
Indiana. Terry Munson visited our facility within just a couple days to
review our process and also make arrangements to have some tests performed
of which CSL would analyze. To make a long story short, CSL provided the
detail analysis that gave objective/empirical evidence that there was no
contamination. In addition the response was very fast which the customer
liked. The point I am trying to make is CSL/Terry provided the information
needed, regardless of who was right or wrong in the ongoing debate, so we
could react properly to our customer. In this particular case there was no
contamination issue and the customer was satisfied that we were able to
produce the evidence to prove that which then gave them the warm fuzzy
feeling they were looking for.
You can reach CSL pretty fast by e:mailing [log in to unmask]
<mailto:[log in to unmask]> and brief Terry Munson on the issue.
Ron Hollandsworth
ITT A/CD
************************************
If this email is not intended for you, or you are not responsible for the
delivery of this message to the addressee, please note that this message may
contain ITT Privileged/Proprietary Information. In such a case, you may not
copy or deliver this message to anyone. You should destroy this message and
kindly notify the sender by reply email. Information contained in this
message that does not relate to the business of ITT is neither endorsed by
nor attributable to ITT.
************************************
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|