By eliminating thermals at via locations you significantly increase
the probability of creating pink ring. Depending on who you talk to
will determine if pink ring is a functional defect or not. If your
finished specification for your board manufacturer states "No pink
ring allowed" you are setting him up for failure. If pink ring is a
non issue with your company and this is reflected in your
specification this is a non issue. The diameter of the center pad,
width of the spokes and diameter of the clearance around the center
pad are significant factors that contribute to the amount of pink ring
present.
***************************************************************************