Honestly,
I've never had to clean the preheat section. However, the vapor chamber is
where I've spent most of my time. You'll get flux residue on the walls, and
a nice green "algae-ish" stuff on the cooling coils. And you're right, it is
NOT fun to clean. I wouldn't try the Easy-Off either, it just makes more of
a mess than anything. I definitely clean more often then 200 hours.
I would imagine the 230 fluid you have is for 63/37 soldering.
BTW, I tried looking fluid that went higher than 260 (for HMP paste). I
couldn't find any.
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 11, 2006 1:19 PM
To: TechNet E-Mail Forum; Jason Gregory
Subject: RE: [TN] RD Technologies Vapor Phase Users
Hi Jason!
We have some of the same fluid as you, although we have some LS-230 too (not
quite sure why that fluid is there...need to ask some questions about that.
I read the manual and it said the vapor chamber should be cleaned every 200
hours of operation, is that what you've found too? Or should it be cleaned
more (or less) often? Also, is the vapor chamber what gets most dirty? Or
does the area around the preheat panels get dirty too?
Looking at the machine, I can see that it is going to be a pain to clean
everything down inside the vapor chamber as they state in the manual.
Kind regards,
-Steve Gregory-
Senior Production Engineer
OAI Electronics
6960 East 12th Street
Tulsa, Oklahoma 74112
(918) 836-0507
(918) 706-2779 CELL
(918) 836-0184 FAX
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, April 11, 2006 12:38 PM
To: [log in to unmask]
Subject: Re: [TN] RD Technologies Vapor Phase Users
Hi Ramon,
Pros:
-Ability to process problematic high temp boards (thicker than .063", high
layer counts, etc.) and not have to jack with as many variables as in
convection or IR -Excellent thermal equilibrium across the assembly and not
having to worry about shadowing or thermal thieving -Probing your board to
determine preheat and then knowing your peak area's temp already and looking
through a little window to observe reflow and giving an extra 15 or 20
seconds over for wetting
Cons:
-Fluid is expensive and if you have excess dragout, you will notice
financially. Fluid is about $1000/gallon -Higher than usual expectations for
tombstoning if your board design is a little lopsided (heavy ground planes
connected to one side of passives) or if your process is a little off.
-Machine is a booger to clean
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Tuesday, April 11, 2006 11:36 AM
To: [log in to unmask]
Subject: Re: [TN] RD Technologies Vapor Phase Users
Hi Jason:
I believe that Vapor phase has a lot of good merits.
Could you share your experience with the machine? Pros and Cons.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Tuesday, April 11, 2006 12:13 PM
To: [log in to unmask]
Subject: Re: [TN] RD Technologies Vapor Phase Users
Hello Steve,
We have a RD here and we use Galden HS-260
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)594-0602 cell
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, April 11, 2006 10:33 AM
To: [log in to unmask]
Subject: [TN] RD Technologies Vapor Phase Users
Mornin' All!
I've just got the opportunity to work with a new vapor phase reflow system
here at my new position. It's a RD Technologies RD3 with a vapor recovery
system. We're in the process of hooking it up, we haven't yet started it up.
I worked with a vapor phase many years ago (1988), and this system is much
nicer than what I remember about the system I worked with in the past.
I was wondering if there are any RD Technologies users out there that have
any "words of wisdom" that they might share with me about the system I'm
that going to be working with. BTW, we're going to using Galden heat
transfer fluids.
Kind regards,
-Steve Gregory-
Senior Production Engineer
OAI Electronics
6960 East 12th Street
Tulsa, Oklahoma 74112
(918) 836-0507
(918) 706-2779 CELL
(918) 836-0184 FAX
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|