Subject: | |
From: | |
Reply To: | |
Date: | Wed, 25 Jun 1997 11:13:39 -0700 |
Content-Type: | TEXT/PLAIN |
Parts/Attachments: |
|
|
We have used HALT/HASS on one product to evaluate our first use of intrusive
solder. Although the testing was only done on a couple of boards, we picked what
we thought were visually "worst-case" intrusive solder joints. We could not
make any of them fail.
On Wed, 25 Jun 1997 05:42:11 -0700 [log in to unmask] wrote:
> From: [log in to unmask]> Date: Wed, 25 Jun 1997 05:42:11 -0700
> Subject: HALT / HASS physical stress systems
> To: [log in to unmask]
>
> Greeetings all,
> I would like to know if anyone has experience or "first-hand"
> information with either the HALT(highly acelerated life tests) and /or
> the HASS (highly accelerated stress screens) techniques developed by
> a company called QualMark. I am interested in reliability testing of
> through hole devices soldered by intrusive soldering techniques.
> Thanks to anyone who may be able to provide information.
> Jay Hinerman
> [log in to unmask]
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|