Russell,
I was my understanding that hard gold, acid, mixed with solder would
create a GALVANIC CELL.
No quite sure how this hard gold is being used.
victor,
-----Original Message-----
From: David Douthit [mailto:[log in to unmask]]
Sent: Thursday, November 14, 2002 5:50 PM
To: [log in to unmask]
Subject: Re: [TN] gold solderaility
Russell,
Be careful!!
You might have "black pad" solder joint issues due to problems with the
nickel bath.
(see archives!)
David A. Douthit
Manager
LoCan LLC
Russell Burdick wrote:
> Hello everyone!
>
> I could use some help concerning soldering to gold.
>
> Problem:
> A customer of ours has given feedback to our salespeople that hard gold
> boards we made in May 2002 were much better to solder to than what we sent
> in October 2002. Biggest difference was stated as the newest boards have
> fiducials that auto pick and place equipment can't read because under the
> lights they look "black". Under normal shop lights both boards look bright
> and shiney(sp?).
>
> Also, the customer commented that on the boards with "black" unreadable
> fiducials had solderjoints that looked very dull.
>
> Known manufacturing/processing differences between months of May and
October
> (aka, confessions of a process engineer):
> Prior to August 2002, dull plated gold boards were scrubbed to improve
> appearances. After August 2002 no scrubbing needed when a carbon treat and
> proper wetters were performed/maintained in nickel and gold baths.
>
> Any and all comments are greatly appreciated.
>
> _________________________________________________________________
> Help STOP SPAM with the new MSN 8 and get 2 months FREE*
> http://join.msn.com/?page=features/junkmail
>
> ---------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|