RMA flux can be removed in a batch-type cleaner using Bioact EC-7 with
isopropyl alcohol, followed by an IPA/water rinse. Omegameter testing
verifies cleanliness.
It can be removed in an inline cleaner using Enviro-Gold 819
neutralizer/soaponifier.
Pat Hogue
Materials and Processes Engineering
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################