We are experiencing problems with a Hewlett Packard PIN diode component
during wave soldering
The HP part is a HSMP-3810 in low profile SOT-23 package (marking EOL) If
the component is Hand soldered it performs to it's specifications. If it is
IR re-flowed the part suffers form a performance degradation (not complete
failure)
HP has refused ( is either unwilling or unable) to provide a preferred
soldering profile for this part
Has one experienced this problem with other low profile SOT-23 type device,
or knows of a IR profile that can be safely used with this part.

Regards

Carey Ritchey


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2