LG 1000 is a b stage modified acrylic adhesive impregnated woven glass
fabric . It is made by duPont and is used primarily as a heat sink bonding
material where resistance to distortion in the bonding film is wanted. It
is according to duPont's data sheet 65 +/- 10% resin and presses 5 +/-10%
mils per ply.The glass fabric is 108 ( probably really 1080 now). Max flow
is given as 5 mils My data sheet is from 1990 but at that time an address
for them was 14 T.W.Alexander Drive , Reasearch Triangle Park N.C.
Phone 919- 248-5000.
----------
From: [log in to unmask]
To: [log in to unmask]; [log in to unmask]; [log in to unmask]
Subject: Pyralux Lg-1000
Date: Friday, September 06, 1996 4:02PM
To Whomever...
Is there anyone out there who is familiar/knowledgeable with a
material used as pre-preg called PYRALUX Lg-1000 ( don't know if
that's a company name or the product). Any help will be appreciated.
Thanks in advance.
Bob Vanech
(203) 852-4810
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|