Good morning everyone,
Lately, we are experiencing solder balls on the top side of single
side PWB. There are some holes that do not get any components before
wave solder. When the board hits wave, it makes "frying" noise and
next thing you see is solder balls. There are two bottom pre-heaters
set at 450 F & 475 F. Solder temp is 500 F. Conveyor speed is 6
fpm.
This problem occurred in the past and was solved by increasing
pre-heat temps. which were originally 325 F & 350 F. Now we are at
the peak of highest component heat ratings. I checked several boards
and made sure that there is no flux left on the bottom side before it
hits solder wave.
Any suggestion on what should I try next will help.
Thanks in advance,
Paresh Patel
Oneac Corp.
(847)816-6000 X-704
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|