Hi I am having solder short defects on the bottom side with SMD devices that
run through the Wave solder. May you let me know any IPC guildelines about
the spacing, orientation or any other design guidelines for avoid solder
defects with SMD devices for double side boards that run through wave
solder.
Thanks David
---------------------------------------------------