I beleive the gold is more porus than HASL, and therefore would not
withstand the sea air as well as HASL. You could build the product with
a no-clean paste, and they say once the left over residue has cured it
acts like a conformal coat.
Good Luck,
Kathy Palumbo
> ----------
> From: Evan Jones[SMTP:[log in to unmask]]
> Sent: Thursday, February 26, 1998 10:18 PM
> To: [log in to unmask]
> Subject: [TN] corrosivity HASL v GOLD
>
> One of our Engineers has asked me to pass on a question. How does the
> corrosion
> resistance of Electroless gold over Nickel (gold thickness of around
> 7
> microinch) compare to horizontal HASL? The target environment is a
> marine type
> environment (salt spray). The customer does not wish to conformally
> coat the
> end product. If anyone has any experience or data in this area I would
> be most
> grateful.
>
> Regards Evan
>
> Evan Jones
> Manufacturing Engineer
> Bluegum Technology
> Ph 61 3 5720 2539 Fax 61 3 5720 2412
> Email [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|