I think what your customer wants is G-10 which is the Non-Flame
retardant version of FR-4. It it usually used in applications
were outgassing of the flame retarding agent is considered to be
more of a risk than PCB/PWB fires.
Frank Firmpong D2D.
***************************************************************************