The best method would be to place the boards into an immersion tin bath.
The immersion tin bath is acidic and will remove any oxide/hydroxide finish
from the surface. For over 40 years immersion tin has been used in the
electronic industry. One of its uses was to "refresh" a solder surface. Oxide coated
tin/lead finishes were cleaned and recoated with a thin coating of tin. In
this application it will easily refresh yours. You might want to consider
using one of the new "immersion white tin" chemistries since they will coat any
exposed copper that might have appeared. .
Rich Edgar
Tec-Line Inc.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------