That's a great story, can you refresh the audience on the history of the
Nauga as well?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, February 27, 2009 11:28 AM
To: [log in to unmask]
Subject: Re: [TN] NTC - Weird one - bismuth in overmold
I will have everyone know that Hillman stole that one from me.
To clarify, "mummy dust" is a generic term used for the secret
ingredients that flux manufacturers add to fluxes to make it work right.
Similar to powdered bats wing and newts nose. You will see it listed on
an MSDS by it's alternative term "Proprietary".
Now I feel obligated to tell the story of the Origin of the Stort and
Snark.
Back when I was in college, and mammoths roamed the earth at the
University of Wisconsin (behold the power of cheese), I was in an
advanced math course - Systems of Linear Differential equations. Which
was a combination of linear algebra and differential equations. Taking
the course with me were my good friends Sue Ross and Morgan Culver. We
three were the only three engineers in a class of 25 students, the rest
being pure math majors. The teacher was a very good one. We were
working on a classic population rise and fall problem involving foxes
and rabbits. In general, as the rabbit population rises so does the fox
population.
Cyclical in nature, dynamic with time. All would have been fine, except
for we 3 engineers. We kept interjecting comments like, rabbits don't
behave like that, or why wouldn't the foxes travel to the adjacent
county where there are plenty of rabbits, rather than die, what happens
if two foxes share one large rabbit. Essentially destroying all the
underlying assumptions and boundary conditions. It frustrated the hell
out of the professor. Finally, in a fit of annoyance, he declared that
he was changing the name of the predators to Storts and the name of the
prey to Snarks, and since none of the smart ass engineers in the class
know the characteristics of a Snark or a Stort, we could then proceed
with the problem. Without missing a beat, Morgan said "I know what a
Stort is - it is a heavyset lowland bird, comprised mainly of meat and
feathers, which flies in ever-diminishing circles crying Wango Wango".
The teacher just stared at us for a minute, then, without a word, walked
out of the classroom. Class dismissed.
So Dave was close, but now you know the rest of the story.
Doug Pauls
Rockwell Collins
Genny Gibbard <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
02/27/2009 10:56 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Genny Gibbard
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] NTC - Weird one - bismuth in overmold
I just about snorted coffee out my nose reading this one. Top marks for
a Friday response!
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: February 27, 2009 10:52 AM
To: [log in to unmask]
Subject: Re: [TN] NTC - Weird one - bismuth in overmold
Hi Ken - ok, in the spirit of Friday, here is the definition of "mummy
dust":
Mummy Dust: noun, derived from old Iowan and Wisconsinian, a slightly
grey powder substance produced by boiling the nests of storts. A stort
is a heavy set low land bird, comprised mainly of meat and feathers,
which flys in ever diminishing circles, crying "Wango, Wango". Storts
belong to the Nauga family.
Dave
Ken Bloomquist <[log in to unmask]> Sent by: TechNet
<[log in to unmask]>
02/27/2009 09:23 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to Ken Bloomquist
<[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [TN] Weird one - bismuth in overmold
OK Dave, I've been waiting for Friday to ask the question; What is
"mummy
dust"? That is one technical term that I've not heard before. Maybe it's
because I live and work on a small island in Washington State and the
dust
hasn't made it this far ;-)
KennyB
-----Original Message-----
From: David D. Hillman [mailto:[log in to unmask]]
Sent: Thursday, February 26, 2009 9:42 AM
To: [log in to unmask]
Subject: Re: [TN] Weird one - bismuth in overmold
Hi Vlad - Nope, based on the huge amount of testing of products for RoHS
materials, it is amazing on how much "mummy dust" is incorporated into
products for specific reasons.
Dave
[log in to unmask]
02/26/2009 11:37 AM
Please respond to
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|