Dirk,
You should also check out IPC-9501 and IPC SM 786A ??
Thanks
Mike Yuen
[log in to unmask]
----------
From: TechNet-request
To: Dirk_Bellamy
Cc: TechNet
Subject: Re: Moisture Sensitivity
Date: Friday, June 28, 1996 9:23AM
Dirk, have a look at the 1995 ECTC proceedings, for an excellent paper by R.
Shook and others. From memory, a portion of this paper looked at the
moisture
absorbtion/desorbtion from components that were moved from ambient
conditions to a dry box, a number of times. If you are trying to set up a
factory policy, I think this will be of use.