Many passive components, also used for hybrid applications (adhesive attachment) had/have Au over Ni termination.
For SMD work, I would not procure that termination if at all possible.
Serhat, you could put a dot of non-conductive adhesive under them, but I still would be concerned about the joint composition ...
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Monday, March 28, 2016 7:25 AM
To: [log in to unmask]
Subject: Re: [TN] smd components with gold over nickel barrier
To avoid confusion I believe you are referring to the PCB?? For enig
> On Mar 28, 2016, at 5:17 PM, Serhat Hasipek <[log in to unmask]> wrote:
>
> Hi to all,
>
> I need to get an information about reflow profile of smd components with gold over nickel barrier. We have encountered tombstoning problem at surface mount capacitances and resistors with gold over nickel barrier. We have applied usual lead free reflow profile with max 245 °C.
> Is there any suggestion to prevent tombstoning at these components except for bonding?
>
>
> Best regards
>
> SERHAT HASİPEK
>
>
> ######################################################################
> Dikkat:
>
> Bu elektronik posta mesaji kisisel ve ozeldir. Eger size
> gonderilmediyse lutfen gondericiyi bilgilendirip mesaji siliniz.
> Firmamiza gelen ve giden mesajlar virus taramasindan gecirilmekte,
> guvenlik nedeni ile kontrol edilerek saklanmaktadir. Mesajdaki
> gorusler ve bakis acisi gondericiye ait olup Aselsan A.S. resmi gorusu
> olmak zorunda degildir.
>
> ######################################################################
> Attention:
>
> This e-mail message is privileged and confidential. If you are not the
> intended recipient please delete the message and notify the sender.
> E-mails to and from the company are monitored for operational reasons
> and in accordance with lawful business practices.
> Any views or opinions presented are solely those of the author and do
> not necessarily represent the views of the company.
>
> ######################################################################
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|