(Thanks to technet for the reactions on my questions on aqueous/IPA cleaning
and assembly carriers)
Question :
Is the "stencil-life" of solder pastes with water soluble flux really that
bad? Can someone give me some practical data (hrs, batch-size, stencil-type,
paste-manufacturur etc)? (...data, data, need more input...)
Thanks again!
*******************************
Ivo de Rooij
Process Engineer
Surface Mount Assembly
Fokker Elmo BV
P.O. Box 75
4630 AB Hoogerheide
The Netherlands