Hey y'all,

We are having solder bridging problems on .5mm pitch SMD quad packages.
We use an .012 wide pad. This results in .0077 spacing between pads
I would like to know what pad sizes others are using as well as paste 
stencil opening size and thickness. 

Thanks,

Dan Ratcliff
Principal PCB Designer
Paradyne Corporation
Largo, FL
813-530-8762
[log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2