Does anyone have information on how to repair gold edge connectors which
have solder on them? I remember a product or service from the late 70's or
early 80's which purported to fix this. Can anyone shed some light on the
subject? I have seen the defect repaired by reflowing with Au80/Sn20 but I
am unsure of the long term reliability of this method.
Thanks,
Denis Meloche
Heraeus Inc
610-825-6050
***************************************************************************