geez, tsk, tsk, that calcium looks like hard water water to me.
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, May 04, 2004 6:53 AM
To: [log in to unmask]
Subject: Re: [TN] Crystalline growth across a capacitor...the next stage
Hi Ray!
I've posted your EDX up on my page too...
-Steve Gregory-
> Guys
>
> Great stuff! Did you find source?
>
> I’ve attached the EDX that was done on the area.
>
> Ray Alberty
>
> Quality Engineer
>
> Telematics and Homelink
>
> Jabil Circuit
>
> 3800 Giddings
>
> Auburn Hills, MI 48326
>
> Phone:248-292-6152
>
> Pager: 248-407-1909
>
> Fax: 248-292-6903
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------