James,
The Navy has a publication in 1983,see MIL-I-46058 conformal coating that
gives paraxylene first epoxy next, polyurethane. Acrylic, RTV and carnish
are poor choices.
Richard
-----Original Message-----
From: James A Larson <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Monday, August 03, 1998 4:51 PM
Subject: [TN] Pacovia Alternative
>Does anybody know of an alternative to Pacovia as a conformal
>release sheet for Blind via processing. Need a material that will
>allow resin to fill but keep off of the surface both etched and
>foil.
>
>Jim Larson
>Johnson Matthey Semiconductor Packages
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|