Hi Bogert:
It seems that as Michael says it may be labor intensive but it
can be done. The land is removed and a larger land with a trace
attached is glued to the substrate and overlapped solder on to the
existing track. Estimate about 2 bucks per land.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Michael McMonagle
Sent: Tuesday, November 22, 2005 8:09 AM
To: [log in to unmask]
Subject: Re: [TN] Making existing PWB land areas larger
Bogert,
Are the pads too small to make contact at all or too small to
provide a proper fillet at the ends of the component? If you are making
contact between the pad and the bottom of the termination, you're
probably better off to just leave it alone as it is. If you can get an
interfacial connection between the pad and the bottom of the component
termination, you can get a physically decent joint that will hold up to
normal usage. Been there, done that. If the product is subject to a
severe use environment, or Class 3, it might not measure up for the long
haul.
The customer designed the board incorrectly; they've got to make
the call. Trying to 'band-aid' a larger pad on to the existing one will
be labor intensive, and will reduce reliability overall. If you've just
got to do it, check out Circuit Technology Center at
http://www.circuittechctr.com/
Mike McMonagle
Quality Engineer
OYO Geospace
7007 Pinemont Drive
Houston, TX 77040
713-986-8650
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of - Bogert
Sent: Tuesday, November 22, 2005 4:27 AM
To: [log in to unmask]
Subject: [TN] Making existing PWB land areas larger
November 22, 2005
Folks we have an OEM who designed a PWB with too small a land area for
mounting a surface mount tantalum chip capacitor. This design does not
allow for replacing the capacitor via manual soldering with an iron
since the part will be damaged if the iron touches the part body. Is
there a way to enlarge the existing land size by some type of solder on
land piece. I know they make such an item that folks use for
replacement of damaged traces. If the lands can be increased in size,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
how does one do this and will a reliable solder connection result?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|