> Ernie:
What kind of pressure/etcher configuration are you running? Are they breaking after developing or
etching?
> Date: Thu, 7 May 1998 13:56:11 -0500
> From: [log in to unmask]
> Subject: tents
>
> We seem to have an issue with tents breaking on large
> holes ( .180 to .250 dia. ) as well as slots, typically .118 x .250.
> No matter whose film we have tried, the tents break. It is not always
> every panel, nor every lot. We have an idea that it may be being
> caused by the developer. Has anyone out there wrestled with this
> problem, and if so how was it resolved. To switch to secondary drill
> would just impact that departments output Any help will be deeply
> appreciated.
>
> Ernie Smith
> Electropac Co. Inc.
>
> e-mail to [log in to unmask]
>
> or on the technet
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|