That's a real stretch that Tin whiskers could be the root cause. Unlikely
that it is.
The laptop is probably Lead free if it were a recent one. Unlikely though
that it failed because it was lead free.
A more likely scenario is the battery went into thermal runaway. A definite
possibility with Lithium ions in laptops and cell phones.
Regards,
LS
-----Original Message-----
From: Otto de Smit [mailto:[log in to unmask]]
Sent: Thursday, June 22, 2006 6:41 AM
To: [log in to unmask]
Subject: Tin whiskers?
Good day all,
I just found this article:
http://www.theinquirer.net/?article=32550
Tin whiskers? Lead free.
Regrads,
Otto
---------------------------------
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
All new Yahoo! Mail "The new Interface is stunning in its simplicity and
ease of use." - PC Magazine
THIS EMAIL AND ANY ATTACHED FILES ARE CONFIDENTIAL AND MAY BE LEGALLY
PRIVILEGED. If you are not the addressee, any disclosure, reproduction,
copying, distribution or other dissemination or use of this communication is
strictly prohibited. If you have received this transmission in error, please
notify the sender immediately and delete this email. It is the policy of ACR
Electronics, Inc. that no legally binding statements, representations or
commitments (collectively statements) may be made by email. Any such
statements must be confirmed either by facsimile transmission or by postal
mail before they will have legal effect. The sender of this email is not
authorised to commit the company in any way and the addressee is hereby
notified of that fact.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|