SMT - will the SnPb parts survive the e
SMT or thru hole or mix?
SMT - will the SnPb parts survive the elevated reflow temp for Pb-F?
Thru - you'll contaminate your Pb-F bath with lead
Nothing really stopping you though but don't see it proves much unless
everything is Pb-F/RohS compliant and process compliant.
Japanense "Green leaf" products were/are I believe built this way when
Pb-F parts were not available.
Regards,
Chris
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Larry Koens
Sent: 16 March 2005 14:33
To: [log in to unmask]
Subject: [LF] soldering SnPb components with lead free solder
Leadfree netters,
I have a customer who wants us to build a board to help him validate
lead free. He has a partial mix of components (some are lead free,
others are SnPb). Would it be ok to solder the SnPb components using
lead free solder? I know and understand the product will not be RoHS
compliant, but this is for internal study and not to be marketed.
thanks,
Larry
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you are not
the intended recipient, delete this message. If you are not the intended
recipient, disclosing, copying, distributing, or taking any action based on
this message is strictly prohibited.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|