Chris
What i find amazing is that the exemption report will come out in July,
after the RoHS compliance date. So that means if you've applied for an
exemption you have effectively 'unofficially' gained a stay of execution
whether its granted or not. We'd all like 6 months more, but the majority
of blue-chip companies have worked very hard to get to July only to find
that there are a number of other less scrupulous companies who have taken
the option to just look for excuses. What is the NWML view on this? and
how will they police the exemptions??
That's apart from the China RoHS report which reads 'we are nearly ready
but not'
All stems from no real steering committee in the first place
just having a rant!!
regards
Paul
Paul R Taylor
Senior Engineer, RoHS Compliancy Group, IED
Pitney Bowes Ltd
The Pinnacles, Elizabeth Way, Harlow, Essex, CM19 5BD
tel: +44 1279 449 744 fax +44 1279 449 594
email: [log in to unmask] website: www.pb.com
"James, Chris" <[log in to unmask]>
Sent by: Leadfree <[log in to unmask]>
27/02/2006 12:38
Please respond to
"(Leadfree Electronics Assembly Forum)" <[log in to unmask]>; Please respond
to
"James, Chris" <[log in to unmask]>
To
[log in to unmask]
cc
Subject
Re: [LF] DTi - unofficial note
Works for me - cut and paste it into your browser:
http://www.dti.gov.uk/sustainability/weee/TAC_15Feb06.pdf
Just spotted the error there was a space at the end before the > - now
correct:
<http://www.dti.gov.uk/sustainability/weee/TAC_15Feb06.pdf>
Regards,
Chris
____________________________________________________
Chris James
Engineering Services Manager
Dolby Laboratories, Inc.
ddi: 01793 842136
mob: 07779 854829
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Des Gayler
Sent: 27 February 2006 12:40
To: [log in to unmask]
Subject: Re: [LF] DTi - unofficial note
Hi Chris that appears to be a dead link?
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of James, Chris
Sent: 27 February 2006 12:25
To: [log in to unmask]
Subject: [LF] DTi - unofficial note
The UK Department of Trade and Industry have posted an "Unofficial note"
of the meeting of the "Technical Adaptation Committee on the WEEE and RoHS
Directives" held in Brussels on 15 February 2006.
You will find it on their web
<http://www.dti.gov.uk/sustainability/weee/TAC_15Feb06.pdf >
The report gives a some insight on what is happening about allowing or
denying the various RoHS exemption applications that are in the pipeline.
The Commission has engaged the Öko-Institut to review the 50 or so
exemption requests that it has received since the completion of the first
stakeholder consultation exercise in February last year. The Öko-Institut
is reporting on a monthly basis to the Commission, which then decides
whether to put specific exemption proposals to the TAC for vote.
The Commission proposed the adoption of six new exemptions but - following
discussions with Member States - withdrew one of these. A Qualified
Majority Vote was reached on the remaining five.
The meeting report also has details of a discussion on the interpretation
of "Fixed Installation".
-----------------------------------------
This message (including any attachments) may contain confidential
information intended for a specific individual and purpose. If you
are not the intended recipient, delete this message. If you are
not the intended recipient, disclosing, copying, distributing, or
taking any action based on this message is strictly prohibited.
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee
Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-------------------------------------------------------------------------------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|