Roland,
Thanks! This is exactly the type of story I am looking for.
Bev
----- Original Message -----
From: Leadfree <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon May 12 15:44:25 2008
Subject: Re: [LF] Looking for RoHS stories
Hi Bev
We have found Cr6 as an anti-fingerprint treatment on stainless steel
refrigerators. It is transparent in that application and came as a complete
surprise. As it is applied over stainless steel that has a high Cr0 content
it is virtually impossible to test by screen testing. This was discovered by
querying the supplier.
kind regards
Roland Sommer
Managing Director
RoHS-International
Cell +64 21 716 208
Fax +64 3 3255 031
Skype: rolandsommer (video enabled)
www.rohs-international.com
Have you downloaded our new REACH - Simplified Guidance Notes for Article
Producers yet? Condensing 3000 pages of information into 29 pages and took
400 hours in the making!
Disclaimer. The contents of this email are informational only.
RoHS-International is not a law firm and the contents of this email should
not be construed as legal advice. Please contact your attorney if you
require legal advice.
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Bev Christian
Sent: Tuesday, 13 May 2008 7:15 a.m.
To: [log in to unmask]
Subject: [LF] Looking for RoHS stories
LeadNetters,
I am sending this appeal to both TechNet and Leadfree.
I am writing a paper about the "stories" of RoHS testing. So I am
soliciting for interesting tidbits or full length novels that you would be
willing to share. No names of people, companies or products would of course
be used or shared with anyone else without your written permission.
For instance:
1) Has ANYONE found any mercury or cadmium in supposedly RoHS compliant
components?
2) We've found Cr(VI) - in LEATHER!
Regards,
Bev
RIM
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Leadfree To temporarily stop/(start)
delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
----------------------------------------------------------------------------
---
__________ NOD32 3093 (20080512) Information __________
This message was checked by NOD32 antivirus system. http://www.eset.com
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|