I have been cycling some bare test boards to the JEDEC 020 spec for lead
free reflow trials. I have noticed a tendency for early de-lamination of
areas of the board with copper flood fill on the surface.
This is only occurring after extended cycling, and I have the same effect
from 3 different board manufacturers using 3 different high temperature
laminate constructions.
Anyone else noticed this??
John