I wouldn't worry too much about the gold thickness but suppliers usually
section to demonstrate suitable control of nickel thickness. Thin nickel
causes terrible problems.
Is there a pcb supplier out there?
Rex
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: 13 March 2007 11:18
To: [log in to unmask]
Subject: [LF] PCB plating Qualification
Dear Members,
Is anybody out there looking at statistical data (control charts, Cp,
Cpk values) of plating thicknesses processes for say, ENIG and
evaluating your board house/s on it? Are there any procedures (IPC or
otherwise) for doing so? what matrices can be reasonably achieved for
plating processes? If this analysis is looked it, is it just a one time
deal or is this a recurrent activity (like every 6 months or 1 year or
some other time period)
Wanted to know the general trend in the industry.
Thanks in advance,
Amol
CONFIDENTIALITY NOTICE:
This e-mail, and any attachments, is for the sole use of the intended
recipient(s) and may contain information that is confidential and
protected from disclosure under the law. Any unauthorized review, use,
disclosure, or distribution is prohibited. If you are not the intended
recipient, please contact the sender by reply e-mail, and delete/destroy
all copies of the original message and attachments.
Thank you.
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d To unsubscribe, send a message to [log in to unmask] with following
text in the BODY (NOT the subject field): SIGNOFF Leadfree To
temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL) Search previous postings at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please visit http://www.messagelabs.com/email
______________________________________________________________________
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|