The BGA will be fine provided you were able to meet reflow temps for the
snpb solder at the center spheres. What you may notice is that the bga
itself may appear elevated (or less collapsed, is that a word?) when
compared to old snpb plastic bgas.
Should be just fine..
-----Original Message-----
From: Carol Spiers [mailto:[log in to unmask]]
Sent: Tuesday, December 07, 2004 12:23 PM
To: (Leadfree Electronics Assembly Forum); Smith, Rick
Subject: RE: [LF] Transition questions, Pb to Pbfree wave soldering ??
Thanks for the input Rick, I totally agree with you. Makes sense since
the two swipe thing would be totally inefficient (costly) as I would
have to mask of the footprints for the leaded parts, put the non leaded
parts in after the first Pbfree swipe and then wave in th SnPb. Now for
my next question.
Here's a real life scenario that I am living with. I now have a board
that is populated with SnPb parts, the component supplier has converted
the BGA to lead free. I had the choice to
a) change my process to high temp SnPb solder at smt (and adjust oven to
higher temp and assume I am still within scope of thermal limits of all
components on board) to help ensure joint reliability or
b) convert the whole smt process to lead free paste and subsequently
adjust ovens to even higher temp, (at this point not sure if thermal
limits on all parts can withstand the potentially 20 Deg C adjustment)
for this product.
I opted to go with
c) ran the BGA in my current process with no adjustments.
We have completed all functional testing with no failures, but, I have
sent samples to a lab for xray and cross sectioning and comparison
evaluations to determine long term reliability.
I haven't received the results back yet.
What would you have done?
Carol
-----Original Message-----
From: Smith, Rick [mailto:[log in to unmask]]
Sent: December 07, 2004 10:39 AM
To: [log in to unmask]
Subject: Re: [LF] Transition questions, Pb to Pbfree wave soldering ??
Team,
?Maybe this is just another duh Rick? If so, you can slap me later at
APEX.
Suggest soldering everything on SnPb wave. LF parts typically solder
fine with SnPb so that will cure all since you won't be LF anyways.
Better to do in one swipe?
The amount of contamination to a LF wave may be insignificant to RoHS,
but maybe not, if the wave has a 1200 lb pot, it currently costs about
$15000.00 to run a pure tin purge and re-fill, so maybe best to leave it
alone until enough data is available to determine how much contamination
could happen??
My thoughts..
Save your wave for the pure stuff
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of MA/NY DDave
Sent: Tuesday, December 07, 2004 11:26 AM
To: [log in to unmask]
Subject: Re: [LF] Transition questions, Pb to Pbfree wave soldering ??
Hi Pratap, Carol, IPC LF Listservers,
<If you have to run mixed parts, FIRST run with PbFree parts on PbFree
wave solder and THEN run with Tin/Lead parts on SnPb wave solder.
Tin/Lead being lower temperature will not flow and therefore will not
contaminate PbFree pot.>
Pratap I think I understand what you are striving to do above, yet I
believe you made a slight error in the soldering temperature heirarchy
or
your process description. Even changing the heirarchy the pot
temperatures
kind of overlap pasty regions so I don't think this will work. YET
reversing the order and doing SnPb component insertion and solder
afterwards is interesting.
Please correct me, as appropriate
Yours in Engineering, Dave
YiEngr, MA/NY DDave
Yours in
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|