text/plain (87 lines)
IMO, as it stands now, this will impact the component mfrs using raw

ingredients rather than product mfrs, but no doubt the powers that be

will twist it to make sure everyone is impacted as much as possible.



Regards,

 

Chris

 



-----Original Message-----

From: Leadfree [mailto:[log in to unmask]] On Behalf Of Paul Jackson

Sent: 30 August 2006 08:50

To: [log in to unmask]

Subject: [LF] REACH



Is REACH going to be like RoHS... what does it mean for the industry as

a whole....? 



http://www.netregs.gov.uk/netregs/legislation/380525/1285481/?lang=_e



 

 

 

Paul Jackson

Hotline Purchasing Manager

Black Box Network Services

Tel: 0118 965 5225

Fax: 0118 9751 565

E-Mail:  Paul <mailto:[log in to unmask]>

[log in to unmask]



Web: www.blackbox.co.uk



One source for worldwide infrastructure services







************************************************************************

*********

One source for worldwide infrastructure services 

Black Box is the world's largest technical services company dedicated to

designing, building and maintaining today's complicated network

infrastructure systems. 

Black Box services clients of all sizes in 141 countries throughout the

world. 

This email and any files transmitted with it are confidential and

intended solely for the use of the individual or entity to whom they are

addressed. If you have received this email in error please notify the

sender by replying to this email. 

This footnote also confirms that this email message has been swept by

MIMEsweeper for the presence of computer viruses. 

www.blackbox.co.uk 

************************************************************************

*********



------------------------------------------------------------------------

-------Leadfee Mail List provided as a service by IPC using LISTSERV

1.8d

To unsubscribe, send a message to [log in to unmask] with following text

in

the BODY (NOT the subject field): SIGNOFF Leadfree

To temporarily stop/(start) delivery of Leadree for vacation breaks

send: SET Leadfree NOMAIL/(MAIL)

Search previous postings at: http://listserv.ipc.org/archives

Please visit IPC web site

http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional

information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100

ext.2815

------------------------------------------------------------------------

-------



-----------------------------------------

This message (including any attachments) may contain confidential

information intended for a specific individual and purpose.  If you

are not the intended recipient, delete this message.  If you are

not the intended recipient, disclosing, copying, distributing, or

taking any action based on this message is strictly prohibited.



-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------

ATOM RSS1 RSS2