On Jun 17, 2010, at 3:30 PM, Wendi Boger <[log in to unmask]> wrote:
> Need clarification on the definition of Via Structures as is relates
> to
> Microsection Requirements.
>
>
>
> 3.6.1.5 Microsection Requirements
>
>
>
> ..... Evaluation of all applicable PTHs and vias, including
> blind and buried, for all such structures found on the finished
> printed
> board shall be inspected in the vertical cross section in accordance
> with Table 4-3. ...
>
>
>
> If a board has 1-2 lasers and 1-2-3 stacked lasers is it correct to
> have 2 coupons one as 1-2 and one as 2-3. Both drill cycles and
> plating
> cycles are represented but the 1-2-3 total via structure is not.
> Seems
> like the 1-2 and 2-3 only is bending the intent.
>
>
>
>
>
> Wendi
>
>
>
>
>
> This communication is for use by the intended recipient(s) only and
> may contain information that is privileged, confidential,
> proprietary and exempt from disclosure under applicable law. You are
> hereby notified that any dissemination, distribution, forwarding or
> copying hereof is strictly prohibited without the express written
> consent of DDi. If you have received this communication in error or
> are not the intended recipient, you should destroy the message and
> any attachments or copies, and you are prohibited from retaining,
> distributing, disclosing, or using any information contained herein.
> Please inform us of the erroneous delivery by return e-mail. Thank
> you for your cooperation.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|