Denise,
Unless I'm mis-reading the specs, I don't think you have a
requirement to do this test unless you're building the specific Type of
product:
6012 Type 1
6013 Types 1 & 5, or when specified
6018 Type 1
The product types for which this is a listed requirement are single sided
or do not contain PTHs.
Thanks,
Lance
From: Denise Chevalier <[log in to unmask]>
To: <[log in to unmask]>
Date: 06/24/2011 08:05 AM
Subject: Re: [IPC-600-6012] Bond Strength Testing for Unsupported Holes
Sent by: IPC-600-6012 <[log in to unmask]>
Thanks Chris - it was not found as a deficiency we reviewed parts
running and there were no designs containing unsupported holes whew!
Need to figure out how to close this gap in our system though.
Do you know if there is a drive to clear up this requirement between
the base spec, IPC-2221 and TM-650?
Denise J Chevalier
Amphenol Printed Circuits
Quality Engineer
Phone - 603-324-4530
Fax - 603-386-6442
CONFIDENTIALITY NOTICE: This email message, including any attachments,
is for the sole use of the intended recipient(s) and contains
confidential and privileged information. Any unauthorized review, use,
disclosure or distribution is prohibited. If you are not the intended
recipient, please reply to the sender by email and destroy all copies of
the original message.
EXPORT CONTROL NOTICE: This email transmission contains information
controlled for export purposes under the U.S. International Traffic in
Arms Regulations (ITAR) and is intended for the recipient only. No
export, sale, transfer, release or other disposition of this information
is permitted without prior authorization from the U.S. Government.
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of Chris
Mahanna
Sent: Friday, June 24, 2011 11:00 AM
To: [log in to unmask]
Subject: Re: [IPC-600-6012] Bond Strength Testing for Unsupported Holes
Denise,
If you have unsupported holes, you'll need to make an A coupon with
unsupported annular rings for test.
I going to assume you don't have unsupported holes, in which case, IF
you are not fearful of false positive nonconformance, you can run SMT
bond strength testing on the N coupon. Of course, both the method and
coupon are "cancelled".
Word of advice: be careful about agreeing to this.
Background: Not that it is necessarily related to your audit, but I
would say there is MUCH increased interest in this subject due to
cratering. But, you have to be very careful about using room temp bond
strength tests for conformance. And it is a very marginal risk
mitigation for cratering.
I would fight the deficiency finding if I were you.
Chris
Chris Mahanna
Robisan Lab
-----Original Message-----
From: IPC-600-6012 [mailto:[log in to unmask]] On Behalf Of John Perry
Sent: Friday, June 24, 2011 10:46 AM
To: [log in to unmask]
Subject: [IPC-600-6012] Bond Strength Testing for Unsupported Holes
Hello Everyone,
I am submitting this query on behalf of Denise Chevalier at Amphenol
Printed Circuits:
We are being audited on 6012, 6013, and 6018; part of the survey
requires unsupported hoes be tested for bond strength monthly - we send
in our A/B coupons but they never test for bond strength saying they are
not required which makes sense because the A/B coupon has plated through
holes. Does the group have a suggested methodology for how they comply
to this testing while still conforming to the base spec and IPC-TM-650?
Denise
Denise J Chevalier
Amphenol Printed Circuits
Quality Engineer
Phone - 603-324-4530
Fax - 603-386-6442
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|