John/Alcon:
- I don't think that there should be an allowance for lifted lands unless the
industry is ready to accept lifted lands as the norm.  It would seem that
lifted lands should continue to be the exception, to be delt with on an
as-required basis between the two (or more) parties involved.
- My two cents.
Jim Moffitt